Fig. S3. Thermal analysis of nanostructured PCL-G nanocomposite (a) TGA showing high thermal stability of the scaffolds till ~300 °C. (b) DSC graph indicating a decrease in the melting temperature of PCL nano-fibres from 60.1 to 55.4 °C after the addition of small amount of G. (c,d) Tensile stress-strain curves of PCL and PCL-G nanocomposite indicating an increase in tensile strength with increasing concentrations of G.

Funding

This work was funded by the Department of Biotechnology, Govt. of India (BT/01/COE/07/03) India. We are also grateful for the support of the All India Institute of Medical Sciences, New Delhi.

History

Usage metrics

    Nanomedicine

    Exports

    RefWorks
    BibTeX
    Ref. manager
    Endnote
    DataCite
    NLM
    DC